The Work is still in progress in this new DSpace server.
 

Flexural strength of dental porcelains with thermocycling and different firing protocols

dc.contributor.authorArRejaie, Aws
dc.date.accessioned2016-10-11T12:15:20Z
dc.date.accessioned2021-03-31T10:39:44Z
dc.date.available2016-10-11T12:15:20Z
dc.date.available2021-03-31T10:39:44Z
dc.date.issued2014
dc.descriptionpages 202-206
dc.description.abstractThis is an in vitro study comparing the flexural strength of two dental porcelain after thermocycling, repetitive multiple firings and peak firing temperature (PFT) modifications. <b>Materials and Methods:</b> Two types of dental porcelains were used in this study: Cercon® Cream Love and Cercon® Cream Kiss (DeguDent, Hanau-Wolfgang/Germany). A total of 50 specimens per porcelain were divided into five groups with ten specimens per group. The first group was fired following the manufacturer's recommendations (control). The second group was fired 10 times repetitively, and the third group was fired and then exposed to 3000 episodes of thermocycling. The fourth group was fired with the PFT modified by + 10°C. The last group was fired with the PFT modified by −10°C. All specimens were tested for flexural strength with the three-point bending test using a universal testing machine (Instron) with a crosshead speed of 0.5 mm/min. <b>Results:</b> The flexural strength, mean (standard deviation [SD]) MPa, of Cercon® Ceram Kiss were: Control, 59.6 (7.82); 10 firings, 82.37 (26.32); thermocycling, 68.93 (9.55); PFT (+10°C), 75.28 (5.63); and PFT (−10°C), 75.94 (2.85). The results for the flexural strength, mean (SD), of Cercon® Ceram Love were: Control, 59.33 (9.9); 10 firings, 106.07 (28.43); thermocycling, 69.87 (11.17); PFT (+10°C), 65.7 (10.46); and PFT (−10°C), 51.1 (16.56). <b>Conclusion:</b> There was no difference in the flexural strength between the two veneering porcelains. In addition, repetitive firings significantly improved the flexural strength of both porcelains. Thermocycling significantly increased the flexural strength of both porcelains. There were no significant differences in the flexural strength when changing the PFT for Cercon® Ceram Love. Increasing and decreasing the PFT significantly increased the flexural strength of Cercon® Ceram Kiss.
dc.identifier.issn1658-631X
dc.identifier.urihttp://www.sjmms.net/text.asp?2014/2/3/202/142554
dc.identifier.urihttps://repository.iau.edu.sa/handle/123456789/7446
dc.titleFlexural strength of dental porcelains with thermocycling and different firing protocolsen_US
dc.typeArticle

Files